Customization: | Available |
---|---|
Certification: | RoHS, CE |
Composite: | SmCo Magnet |
Still deciding? Get samples of US$ 1.20/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
No Matter you buy 1 pcs or 100,000 pcs of magnets, you can not find better service elsewhere.
SmCo Disc Magnet is made from high performance 26M Sm2Co17.
without other protective coating. The dimension of this item is D10x6mm
magnetized Through Thickness.
Size |
as customer's request |
Shape |
Disc / Round / Disk/ Arc...... |
Material |
Samarium Cobalt |
Grade |
GME-Smco |
Magnetized |
Axial/Radial/Multi-Poles Magnetization |
MOQ |
5000 pcs |
Leading Time |
25-35 working days |
Sample |
Yes |
Certificate |
ISO2000, TS16949, RoHS, CE, SGS & REACH |
Payment |
T/T, PayPal, Western Union |
Material | Grade | Remannence | Coercive Force | Instrinsic Coercive | Max Energy | Density | Temp Coefficient |
Temp Coefficient |
Cuire Temp | Max Working Temp. (TW) |
||||
(Br) | (Hcj) | (Hcb) | (BHmax) | (D) | (Near Br) | (Near Hcj) | (TC) | |||||||
mT | Gs | KA/m | Oe | KA/n | Oe | KJ/m3 | MGOe | g/cm3 | %/K | %/K | ºC | ºC | ||
SmCo 1:5 |
SmCo18 | 840 | 8400 | 605 | 7600 | 1432 | 18000 | 143 | 18 | 8.1 | -0.04 | -0.3 | 750 | 250 |
(SmPr)CO5 | SmCo20 | 890 | 8900 | 637 | 8000 | 1432 | 18000 | 159 | 20 | 8.2 | -0.04 | -0.3 | 750 | 250 |
SmCo22 | 930 | 9300 | 637 | 8000 | 1432 | 18000 | 175 | 22 | 8.2 | -0.04 | -0.3 | 750 | 250 | |
LTc(HM-10) | 590 | 630 | 493 | 6200 | 1430 | 1830 | 80 | 10 | 8.2 | Temp Range | %ºC | 700 | 250 | |
1:5 | 20-100ºC | -0.004 | ||||||||||||
(SmGd)CO5 | 100-200ºC | -0.021 | ||||||||||||
200-300ºC | -0.042 | |||||||||||||
SmCo24 | 980 | 9800 | 676 | 8500 | 1432 | 18000 | 191 | 24 | 8.3 | -0.03 | -0.2 | 800 | 280 | |
SmCo24H | 980 | 9800 | 676 | 8500 | 1989 | 25000 | 191 | 24 | 8.3 | -0.03 | -0.2 | 800 | 280 | |
SmCo26L | 1030 | 10300 | 398 | 5000 | 438 | 5500 | 207 | 26 | 8.3 | -0.03 | -0.2 | 800 | 300 | |
SmCo26 | 1030 | 10300 | 716 | 9000 | 1194 | 15000 | 207 | 26 | 8.3 | -0.03 | -0.2 | 800 | 300 | |
2:17 Sm2 | SmCo26M | 1030 | 10300 | 716 | 9000 | 1592 | 20000 | 207 | 26 | 8.3 | -0.03 | -0.2 | 800 | 300 |
(CoFeCUZr)17 | SmCo26H | 1030 | 10300 | 716 | 9000 | 1989 | 25000 | 207 | 26 | 8.3 | -0.03 | -0.2 | 800 | 350 |
SmCo28 | 1070 | 10700 | 756 | 9500 | 1194 | 15000 | 223 | 28 | 8.3 | -0.03 | -0.2 | 800 | 350 | |
SmCo28M | 1070 | 10700 | 756 | 9500 | 1592 | 20000 | 223 | 28 | 8.3 | -0.03 | -0.2 | 800 | 350 | |
SmCo30 | 1100 | 11000 | 772 | 9700 | 1194 | 15000 | 239 | 30 | 8.3 | -0.03 | -0.2 | 800 | 350 | |
SmCo30M | 1100 | 11000 | 772 | 9700 | 1592 | 20000 | 239 | 30 | 8.3 | -0.03 | -0.2 | 800 | 350 | |
LTc(HMG-22) | 980 | 9800 | 715 | 9000 | 1500 | 20000 | 230 | 23 | 8.3 | Temp Range | %ºC | 840 | 300 | |
2:17 | -50-25ºC | 0.005 | ||||||||||||
(SmEr)2(CoTM)17 | 20-100ºC | 0.012 | ||||||||||||
100-200ºC | 0.006 | |||||||||||||
200-300ºC | -0.025 |
Property | Neodymium | Sm-Co |
Remanence (T) | 1-1.3 | 0.82-1.16 |
Coercivity (MA/m) | 0.875-1.99 | 0.493-1.59 |
Relative permeability | 1.05 | 1.05 |
Temperature coefficient of remanence (%/K) | 0.12 | 0.03 |
Temperature coefficient of coercivity (%/K) | 0.55..-0.65 | 0.15..-0.30 |
Curie temperature (°C) | 320 | 800 |
Density (g/cm3) | 7.3-7.5 | 8.2-8.4 |
CTE, magnetizing direction (1/K) | 5.2×106 | 5.2×106 |
CTE, normal to magnetizing direction (1/K) | 0.8×106 | 11×106 |
Flexural strength (N/mm2) | 250 | 150 |
Compressive strength (N/mm2) | 1100 | 800 |
Tensile strength (N/mm2) | 75 | 35 |
Vickers hardness (HV) | 550-650 | 500-650 |
Electrical resistivity (Ω·cm) | (110-170)×106 | 86×106 |