Customization: | Available |
---|---|
Certification: | RoHS, CE |
Composite: | SmCo Magnet |
Still deciding? Get samples of US$ 4.83/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Size | D1/4"x1/16" |
Shape |
Disc / Round / Disk/ Arc...... |
Material |
Samarium Cobalt |
Pull force |
1.1 pounds |
Magnetized |
Axial/Radial/Multi-Poles Magnetization |
MOQ |
5000 pcs |
Leading Time |
25-35 working days |
Sample |
Yes |
Certificate |
ISO2000, TS16949, RoHS, CE, SGS & REACH |
Payment |
T/T, PayPal, Western Union |
Material | Grade | Remannence | Coercive Force | Instrinsic Coercive | Max Energy | Density | Temp Coefficient |
Temp Coefficient |
Cuire Temp | Max Working Temp. (TW) |
||||
(Br) | (Hcj) | (Hcb) | (BHmax) | (D) | (Near Br) | (Near Hcj) | (TC) | |||||||
mT | Gs | KA/m | Oe | KA/n | Oe | KJ/m3 | MGOe | g/cm3 | %/K | %/K | ºC | ºC | ||
SmCo 1:5 |
SmCo18 | 840 | 8400 | 605 | 7600 | 1432 | 18000 | 143 | 18 | 8.1 | -0.04 | -0.3 | 750 | 250 |
(SmPr)CO5 | SmCo20 | 890 | 8900 | 637 | 8000 | 1432 | 18000 | 159 | 20 | 8.2 | -0.04 | -0.3 | 750 | 250 |
SmCo22 | 930 | 9300 | 637 | 8000 | 1432 | 18000 | 175 | 22 | 8.2 | -0.04 | -0.3 | 750 | 250 | |
LTc(HM-10) | 590 | 630 | 493 | 6200 | 1430 | 1830 | 80 | 10 | 8.2 | Temp Range | %ºC | 700 | 250 | |
1:5 | 20-100ºC | -0.004 | ||||||||||||
(SmGd)CO5 | 100-200ºC | -0.021 | ||||||||||||
200-300ºC | -0.042 | |||||||||||||
SmCo24 | 980 | 9800 | 676 | 8500 | 1432 | 18000 | 191 | 24 | 8.3 | -0.03 | -0.2 | 800 | 280 | |
SmCo24H | 980 | 9800 | 676 | 8500 | 1989 | 25000 | 191 | 24 | 8.3 | -0.03 | -0.2 | 800 | 280 | |
SmCo26L | 1030 | 10300 | 398 | 5000 | 438 | 5500 | 207 | 26 | 8.3 | -0.03 | -0.2 | 800 | 300 | |
SmCo26 | 1030 | 10300 | 716 | 9000 | 1194 | 15000 | 207 | 26 | 8.3 | -0.03 | -0.2 | 800 | 300 | |
2:17 Sm2 | SmCo26M | 1030 | 10300 | 716 | 9000 | 1592 | 20000 | 207 | 26 | 8.3 | -0.03 | -0.2 | 800 | 300 |
(CoFeCUZr)17 | SmCo26H | 1030 | 10300 | 716 | 9000 | 1989 | 25000 | 207 | 26 | 8.3 | -0.03 | -0.2 | 800 | 350 |
SmCo28 | 1070 | 10700 | 756 | 9500 | 1194 | 15000 | 223 | 28 | 8.3 | -0.03 | -0.2 | 800 | 350 | |
SmCo28M | 1070 | 10700 | 756 | 9500 | 1592 | 20000 | 223 | 28 | 8.3 | -0.03 | -0.2 | 800 | 350 | |
SmCo30 | 1100 | 11000 | 772 | 9700 | 1194 | 15000 | 239 | 30 | 8.3 | -0.03 | -0.2 | 800 | 350 | |
SmCo30M | 1100 | 11000 | 772 | 9700 | 1592 | 20000 | 239 | 30 | 8.3 | -0.03 | -0.2 | 800 | 350 | |
LTc(HMG-22) | 980 | 9800 | 715 | 9000 | 1500 | 20000 | 230 | 23 | 8.3 | Temp Range | %ºC | 840 | 300 | |
2:17 | -50-25ºC | 0.005 | ||||||||||||
(SmEr)2(CoTM)17 | 20-100ºC | 0.012 | ||||||||||||
100-200ºC | 0.006 | |||||||||||||
200-300ºC | -0.025 |
Property | Neodymium | Sm-Co |
Remanence (T) | 1-1.3 | 0.82-1.16 |
Coercivity (MA/m) | 0.875-1.99 | 0.493-1.59 |
Relative permeability | 1.05 | 1.05 |
Temperature coefficient of remanence (%/K) | 0.12 | 0.03 |
Temperature coefficient of coercivity (%/K) | 0.55..-0.65 | 0.15..-0.30 |
Curie temperature (°C) | 320 | 800 |
Density (g/cm3) | 7.3-7.5 | 8.2-8.4 |
CTE, magnetizing direction (1/K) | 5.2×106 | 5.2×106 |
CTE, normal to magnetizing direction (1/K) | 0.8×106 | 11×106 |
Flexural strength (N/mm2) | 250 | 150 |
Compressive strength (N/mm2) | 1100 | 800 |
Tensile strength (N/mm2) | 75 | 35 |
Vickers hardness (HV) | 550-650 | 500-650 |
Electrical resistivity (Ω·cm) | (110-170)×106 | 86×106 |